Design Safe Analysis
Verification Tests
Water Exposure test
Please refer to following link for video:
https://drive.google.com/open?id=0B3I2iDuv_3JBdG5DUFBJdjlzZ2c
https://drive.google.com/open?id=0B3I2iDuv_3JBdG5DUFBJdjlzZ2c
Temperature test
45 degrees C before:
https://drive.google.com/open?id=0B9TWw4R7NKqRYjNpNEU4cENZS28
45 degrees C after:
https://drive.google.com/open?id=0B9TWw4R7NKqRNzkyYXF6TF8xRWM
0 degrees C:
https://drive.google.com/open?id=0B9TWw4R7NKqRYjNpNEU4cENZS28
45 degrees C after:
https://drive.google.com/open?id=0B9TWw4R7NKqRNzkyYXF6TF8xRWM
0 degrees C:
- An ABS portion of the splint was placed in a freezer set to 0 degrees C for a period of 30 minutes
- The structural integrity of the ABS was determined to be the same before and after the test
- This is determined by applying a compressive force onto the ABS
- This is determined by applying a compressive force onto the ABS
drop test
drop_test.mov | |
File Size: | 4889 kb |
File Type: | mov |
Breathability
- Breathability was determined subjectively
- User wore splint while performing tasks over a period of four hours
- Comfort level of hand was determined via user feedback and sweatiness level
- User confirmed that breathability was acceptable, though the hypafix layer was getting somewhat sweaty
Installation time
Due to upload size limitations, please refer to following link for video:
https://drive.google.com/file/d/0B9TWw4R7NKqRRW8zanJYNkJFQ3c/view
https://drive.google.com/file/d/0B9TWw4R7NKqRRW8zanJYNkJFQ3c/view
Weight Test
Pressure Test
Due to a lack of proper instrumentation, pressure applied was measured subjectively using user feedback. Users reported that the elastic glove provided a significant, but not uncomfortable, pressure onto their hands.
Working Prototype VIDEO
Due to upload size limitations, please refer to following link for video: